Material Notes:
TRA-DUCT 2916 is an electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require high flexibility coupled with good electrical and mechanical properties. This two-part, smooth paste adhesive of refined pure silver and epoxy resin components is free of solvents and copper or carbon additives. It develops strong, durable, resilient, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic insulates. TRA-DUCT 2916 cures at room temperature and can be used as a flexible "cold-solder" for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, flexible circuits, wave guides, flat cable and high frequency shields. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 2.90 g/cc
2.90 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
Thermal Properties Metric English Comments
Thermal Conductivity 1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 5.00 °C
41.0 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.00060 ohm-cm
0.00060 ohm-cm
cured 5 min @ 160°C
0.00080 ohm-cm
0.00080 ohm-cm
cured 2 hrs @ 65°C
0.00080 ohm-cm
0.00080 ohm-cm
cured 24 hrs @ 25°C
0.0012 ohm-cm
0.0012 ohm-cm
cured 15 min @ 150°C
0.0034 ohm-cm
0.0034 ohm-cm
cured 1 hr @ 110°C
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Color Silver
Mix Ratio, parts by weight 100/115
Resin/Hardener