Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.21 - 1.38 g/cc | 0.0437 - 0.0499 lb/in³ | Average value: 1.29 g/cc Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Average value: 1.35 g/cc Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Density | 1.06 - 1.38 g/cc | 0.0383 - 0.0499 lb/in³ | Average value: 1.18 g/cc Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.15 - 1.38 g/cc | 0.0415 - 0.0499 lb/in³ | Average value: 1.20 g/cc Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Density | 1.30 - 1.38 g/cc | 0.0470 - 0.0499 lb/in³ | Average value: 1.34 g/cc Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m.. |
|||
Density | 1.14 - 1.38 g/cc | 0.0412 - 0.0497 lb/in³ | Average value: 1.25 g/cc Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds RKT 226 Rigid PVC, Extrusion Lead Free Metal effect profiles |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds RKT 736/K1 Rigid PVC, Extrusion Lead Free Transparent profiles |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds SAR 03 Rigid PVC, Antishock Injection Molding Lead Free Electric antishock fittings |
|||
Density | 1.08 - 1.38 g/cc | 0.0390 - 0.0498 lb/in³ | |
Fibre Glast 182 White Gel Coat #182 White Gel Coat is a highly durable ISO gel coat and is the industry production standard for molding applications. Use as a sandable base coat for painting or polish to a high luster finish. Spr.. |
|||
Density | 1.36 - 1.38 g/cc | 0.0491 - 0.0499 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® FB M400 EEA Oxidized Textile Fiber, Milled Fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Density | 1.36 - 1.38 g/cc | 0.0491 - 0.0499 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® FB T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 8318/2 Flexible PVC, Sheathing Lead Free Sheathing coaxial TV cables |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 89/2 Flexible PVC, Insulation Insulation for special application |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds HL 101 Flexible PVC, Insulation for High Temperatures Operating temperature 80°C |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds HLA 075 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds ARC 10 Rigid PVC, Atoxic for General Purpose Bottles medium antishock |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds ARC 20 Rigid PVC, Atoxic for General Purpose Bottles medium/high antishock |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds ARC 30 Rigid PVC, Atoxic for General Purpose Bottles very high antishock |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 75/R Flexible PVC, Flame Retardant Sheathing According to UL 1581 Class 43 (90°C) |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
Fainplast Compounds HL 91 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C |
|||
Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Density | 1.35 - 1.38 g/cc | 0.0488 - 0.0499 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Density | 1.35 - 1.38 g/cc | 0.0488 - 0.0499 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Density | 1.35 - 1.38 g/cc | 0.0488 - 0.0499 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric .. |
|||
Density | 1.04 - 1.38 g/cc | 0.0376 - 0.0500 lb/in³ | Average value: 1.14 g/cc Grade Count:58 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Density | 1.28 - 1.38 g/cc | 0.0462 - 0.0499 lb/in³ | Average value: 1.32 g/cc Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 96 Flexible PVC, Insulation for High Temperatures Lead Free Operating temperature 105°C |
|||
Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/1 Flexible PVC, Sheathing General purposes |