Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00300 cm/cm | 0.00300 in/in | ASTM D955 |
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00300 - 0.0470 cm/cm | 0.00300 - 0.0470 in/in | Average value: 0.0189 cm/cm Grade Count:112 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0140 cm/cm | 0.00300 - 0.0140 in/in | Average value: 0.00582 cm/cm Grade Count:27 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00517 cm/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00450 cm/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Average value: 0.00490 cm/cm Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00557 cm/cm Grade Count:55 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0250 cm/cm | 0.00300 - 0.0250 in/in | Average value: 0.00889 cm/cm Grade Count:11 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00850 cm/cm | 0.00300 - 0.00850 in/in | Average value: 0.00576 cm/cm Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00300 cm/cm @Temperature 80.0 - 80.0 °C |
0.00300 - 0.00300 in/in @Temperature 176 - 176 °F |
Average value: 0.00300 cm/cm Grade Count:2 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0210 cm/cm | 0.00300 - 0.0210 in/in | Average value: 0.0131 cm/cm Grade Count:39 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00700 cm/cm | 0.00300 - 0.00700 in/in | Average value: 0.00518 cm/cm Grade Count:20 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00450 cm/cm | 0.00300 - 0.00450 in/in | Average value: 0.00400 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00537 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0170 cm/cm | 0.00300 - 0.0170 in/in | Average value: 0.00566 cm/cm Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00543 cm/cm Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |