Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00503 cm/cm Grade Count:58 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00537 cm/cm Grade Count:51 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.000800 - 0.00800 cm/cm | 0.000800 - 0.00800 in/in | Average value: 0.00547 cm/cm Grade Count:7 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00552 cm/cm Grade Count:106 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00628 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00455 cm/cm Grade Count:174 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00420 cm/cm Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00800 cm/cm | 0.000500 - 0.00800 in/in | Average value: 0.00304 cm/cm Grade Count:14 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00319 cm/cm Grade Count:7 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00583 cm/cm Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00800 cm/cm | 0.000200 - 0.00800 in/in | Average value: 0.00255 cm/cm Grade Count:21 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00436 cm/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00800 cm/cm | 0.000500 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:101 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00526 cm/cm Grade Count:248 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00468 cm/cm Grade Count:11 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00504 cm/cm Grade Count:104 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00356 cm/cm Grade Count:13 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00420 cm/cm Grade Count:130 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00543 cm/cm Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |