Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00200 - 0.0250 cm/cm
0.00200 - 0.0250 in/in
Average value: 0.00748 cm/cm Grade Count:72
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim..
Linear Mold Shrinkage 0.000 - 0.0250 cm/cm
0.000 - 0.0250 in/in
Average value: 0.00452 cm/cm Grade Count:531
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cm
0.00100 - 0.0250 in/in
Average value: 0.0117 cm/cm Grade Count:36
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.000500 - 0.0250 cm/cm
0.000500 - 0.0250 in/in
Average value: 0.00217 cm/cm Grade Count:18
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Linear Mold Shrinkage 0.000500 - 0.0250 cm/cm
0.000500 - 0.0250 in/in
Average value: 0.0136 cm/cm Grade Count:218
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm
0.0100 - 0.0250 in/in
Average value: 0.0175 cm/cm Grade Count:4
Overview of materials for Polypropylene, Fiber Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage 0.00300 - 0.0250 cm/cm
0.00300 - 0.0250 in/in
Average value: 0.00889 cm/cm Grade Count:11
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.00200 - 0.0250 cm/cm
0.00200 - 0.0250 in/in
Average value: 0.0232 cm/cm Grade Count:13
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Linear Mold Shrinkage 0.00000500 - 0.0250 cm/cm
0.00000500 - 0.0250 in/in
Average value: 0.00407 cm/cm Grade Count:262
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Linear Mold Shrinkage 0.00200 - 0.0250 cm/cm
0.00200 - 0.0250 in/in
Average value: 0.0122 cm/cm Grade Count:10
Overview of materials for Nylon 66, 10% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ..
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cm
0.00100 - 0.0250 in/in
Average value: 0.0131 cm/cm Grade Count:17
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage 0.00800 - 0.0250 cm/cm
0.00800 - 0.0250 in/in
Average value: 0.0131 cm/cm Grade Count:11
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.0130 - 0.0250 cm/cm
0.0130 - 0.0250 in/in
Average value: 0.0169 cm/cm Grade Count:5
Overview of materials for Nylon 11 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00200 - 0.0250 cm/cm
0.00200 - 0.0250 in/in
Average value: 0.0118 cm/cm Grade Count:23
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Linear Mold Shrinkage 0.000700 - 0.0250 cm/cm
0.000700 - 0.0250 in/in
Average value: 0.0183 cm/cm Grade Count:29
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Linear Mold Shrinkage 0.00100 - 0.0250 cm/cm
0.00100 - 0.0250 in/in
Average value: 0.0122 cm/cm Grade Count:14
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm
0.0100 - 0.0250 in/in
Average value: 0.0159 cm/cm Grade Count:16
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.0100 - 0.0250 cm/cm
0.0100 - 0.0250 in/in
Average value: 0.0173 cm/cm Grade Count:7
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..