Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000 - 0.0200 cm/cm
0.000 - 0.0200 in/in
Average value: 0.00468 cm/cm Grade Count:268
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Linear Mold Shrinkage 0.000 - 0.0250 cm/cm
0.000 - 0.0250 in/in
Average value: 0.00452 cm/cm Grade Count:531
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Linear Mold Shrinkage 0.000 - 0.00600 cm/cm
0.000 - 0.00600 in/in
Average value: 0.00223 cm/cm Grade Count:50
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00232 cm/cm Grade Count:146
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Linear Mold Shrinkage 0.000 - 0.00900 cm/cm
0.000 - 0.00900 in/in
Average value: 0.00184 cm/cm Grade Count:17
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Linear Mold Shrinkage 0.000 - 0.0300 cm/cm
0.000 - 0.0300 in/in
Average value: 0.00259 cm/cm Grade Count:88
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage 0.000 - 0.0100 cm/cm
0.000 - 0.0100 in/in
Average value: 0.00164 cm/cm Grade Count:50
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.000 - 0.0150 cm/cm
0.000 - 0.0150 in/in
Average value: 0.00533 cm/cm Grade Count:3
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..
Linear Mold Shrinkage 0.000 - 0.00500 cm/cm
0.000 - 0.00500 in/in
Average value: 0.00133 cm/cm Grade Count:40
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.000 - 0.00400 cm/cm
0.000 - 0.00400 in/in
Average value: 0.00126 cm/cm Grade Count:39
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm
0.000 - 0.00200 in/in
Average value: 0.000869 cm/cm Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Linear Mold Shrinkage 0.000 - 0.00300 cm/cm
0.000 - 0.00300 in/in
Average value: 0.00100 cm/cm Grade Count:19
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Linear Mold Shrinkage 0.000 cm/cm
0.000 in/in
Average value: 0.000 cm/cm Grade Count:4
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage 0.000 - 0.0100 cm/cm
0.000 - 0.0100 in/in
Average value: 0.00531 cm/cm Grade Count:104
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm
0.000 - 0.00200 in/in
Average value: 0.000760 cm/cm Grade Count:5
Overview of materials for Phenolic, Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage 0.000 - 0.00600 cm/cm
0.000 - 0.00600 in/in
Average value: 0.00210 cm/cm Grade Count:18
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.000 - 0.0220 cm/cm
0.000 - 0.0220 in/in
Average value: 0.00607 cm/cm Grade Count:207
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Linear Mold Shrinkage 0.000 - 0.0120 cm/cm
0.000 - 0.0120 in/in
Average value: 0.00205 cm/cm Grade Count:38
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage 0.000 - 0.00100 cm/cm
0.000 - 0.00100 in/in
Average value: 0.000449 cm/cm Grade Count:12
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00477 cm/cm Grade Count:49
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Linear Mold Shrinkage 0.000 - 0.0230 cm/cm
0.000 - 0.0230 in/in
Average value: 0.00449 cm/cm Grade Count:704
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Linear Mold Shrinkage 0.000 - 0.0100 cm/cm
0.000 - 0.0100 in/in
Average value: 0.00385 cm/cm Grade Count:79
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
Linear Mold Shrinkage 0.000 - 0.0400 cm/cm
0.000 - 0.0400 in/in
Average value: 0.00583 cm/cm Grade Count:27
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..