Mechanical Properties Metric English Comments
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Injection; ISO 527
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Injection; ISO 527
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Injection; ISO 527
Raschig Group DECAL® 1760 Phenolic
Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Injection; ISO 527
Raschig Group DECAL® 2061 Phenolic
Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and ..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Injection and Compression; ISO 527
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Compression; ISO 527
Raschig Group DECAL® 572R Phenolic
Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
Compression; ISO 527
Raschig Group DECAL® 666/8 Phenolic
Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
ISO 527
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
Tensile Strength 40.0 - 70.0 MPa
5800 - 10200 psi
Injection; ISO 527
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Tensile Strength 50.0 - 70.0 MPa
7250 - 10200 psi
ISO 527
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Tensile Strength 40.0 - 70.0 MPa
5800 - 10200 psi
Injection; ISO 527
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Tensile Strength 40.0 - 70.0 MPa
5800 - 10200 psi
Injection; ISO 527
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..
Tensile Strength 40.0 - 70.0 MPa
5800 - 10200 psi
Injection; ISO 527
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..