Material Notes:
Basic grade, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Melt Flow 3.0 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.0 MPa
9570 psi
ISO 527
Elongation at Break 5.0 %
5.0 %
ISO 527
Flexural Strength 108 MPa
15700 psi
ISO 178
Flexural Modulus 4.60 GPa
667 ksi
ISO 178
Charpy Impact, Notched 0.160 J/cm²
0.761 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 170 °C
338 °F
Maximum Service Temperature, Air 240 °C
464 °F
Deflection Temperature at 0.46 MPa (66 psi) 59.0 °C
138 °F
ISO 75
Processing Properties Metric English Comments
Rear Barrel Temperature 150 - 180 °C
302 - 356 °F
Middle Barrel Temperature 160 - 200 °C
320 - 392 °F
Front Barrel Temperature 160 - 200 °C
320 - 392 °F
Nozzle Temperature 150 - 180 °C
302 - 356 °F
Descriptive Properties Value Comments
Appearance Transparent
Users viewing this material also viewed the following: