Polymer Property : Izod Impact, Notched = 1.22 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.600 - 0.650 J/cm
1.12 - 1.22 ft-lb/in
ASTM D256
Loxim 235 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Izod Impact, Notched 0.450 - 0.650 J/cm
0.843 - 1.22 ft-lb/in
IS 13411-1992
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown..
Izod Impact, Notched 0.500 - 0.650 J/cm
0.937 - 1.22 ft-lb/in
IS 13411-1992
Amity Thermosets ATO 1510 Phenolic Molding Glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthMedium copper adhesionColo..
Izod Impact, Notched 0.550 - 0.650 J/cm
1.03 - 1.22 ft-lb/in
ASTM D256
Loxim 830 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries