Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 345 MPa | 50000 psi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
FloMet Fe-3% Si Soft Magnetic Alloy FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
Materion BrushBronze® 630 (AMS 4640) 3.0" - 5.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 630 is an Aluminum-Nickel-Bronze alloy that combines high strength along with resistance to wear under severe loading con.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | |
Materion BrushBronze® 95510 (AMS 4880) Centrifugal Cast 1.0" - 17.0" Information supplied by Brush Wellman Engineered Materials.BrushBronze™ 95510 is an Aluminum-Nickel-Bronze alloy that combines high strength, ductility, and good abrasion resistance under sever.. |
|||
Tensile Strength, Yield | 345 - 414 MPa @Strain 0.200 % |
50000 - 60000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275C High Strength Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | 345 - 414 MPa @Strain 0.200 % |
50000 - 60000 psi @Strain 0.200 % |
|
Materion BrushCAST® 275CT Fine Grain Casting Alloy (As Cast) Pouring Temperature: 960-1035°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescri.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
MetalTek C18100 Chrome Zirc Copper High Conductivity Typical property data from forged samples.Information provided by MetalTekCast UNS C18100; Cast Grade C18100 |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
MetalTek MTEK 175-B Cast UNS C95410 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Annealed |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | 0.2% proof |
Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed Nominal Composition: Ti-0.3 Mo-0.8 Ni Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provid.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 %, Temperature 760 °C |
50000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
Sheet |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | >= 345 MPa @Thickness 16.0 - 35.0 mm |
>= 50000 psi @Thickness 0.630 - 1.38 in |
|
ThyssenKrupp XABO® 355 Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Tensile Strength, Yield | >= 345 MPa @Thickness 16.0 - 35.0 mm |
>= 50000 psi @Thickness 0.630 - 1.38 in |
|
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | 0.2% offset |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Typical |
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | Annealed |
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Stress Relieved Data provided by Carpenter Technology Corporation.This is a soft ferritic material designed for operation in more corrosive environments than tolerated by 18% Cr-Fe Type 430 stainless. This new mat.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
AK Steel ZINCGRIP® FORMABLE 50K / ASTM A1008 class 1 / SAE J1392 050 XLK, Grade 50 Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS) Information provided by AK Steel |
|||
Tensile Strength, Yield | 345 - 517 MPa @Strain 0.200 % |
50000 - 75000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 345 - 517 MPa @Strain 0.200 % |
50000 - 75000 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
Typical; Annealed Plate |
ATI Allegheny Ludlum AL 22™ Nickel-Base Alloy, UNS N06022 AL 22 alloy is a Ni-Cr-Mo alloy that provides outstanding resistance to pitting, crevice corrosion, intergranular attack, and stress corrosion cracking. The combination of Cr, Ni, Mo, and W provide.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allvac® Grade 12 UNS R53400 Titanium Alloy Uses: Industrial components. CPI equipment, heat exchangers, pressure vessels, fittings, tubing.Property values are for samples in the metallurgical condition: 1300°F anneal.Information provided by.. |
|||
Tensile Strength, Yield | 345 MPa | 50000 psi | In rolling direction |
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 17-7™ High Strength Stainless Steel, UNS S17700 Property data below is typical of annealed samples. Available in sheet and strip. For use in high-strength springs, bellows, and aerospace applications.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | >= 345 MPa | >= 50000 psi | |
Materion Nibryl Beryllium Nickel Alloy (Nibryl)-360 Rod and Bar; A (A) Temper; All Sizes (UNS N03360) Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |