Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
|
RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, a.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 50-7078/GY Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
|
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1100-8194 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | ASTM D696 |
Samyang Trirex® SF3200GNH20 Polycarbonate, Reinforced Non Halogen for Printers PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.SF3200GNH20 is a reinforced, non-halogen grade for Printers.Applications: Office Machi.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | ISO 11359-2 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | ISO 11359-2 |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS145 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Syntac® 350 Composite Materials Syntactic Foam Syntac 350 foam is a rigid, high strength composite of epoxy resin and microscopic hollow glass microspheres designed specifically for fabricating thermoforming plugs and other associated tooling. .. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 50.0 - 200 °C |
17.2 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 1031 Polyimide, 40% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also .. |
|||
CTE, linear | 31.0 µm/m-°C | 17.2 µin/in-°F | x direction |
Arlon IsoClad 933 Non-Woven Fiberglass Reinforced PTFE Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
|
Armstrong A-12-T Epoxy Adhesive Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8266G HS is a heat stabilized, 40% glass and mineral reinforced nylon 6 injection molding compound resulting in a balance of engineering properties with excellent dimensional stability, low.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
17.2 µin/in-°F @Temperature -40.0 - 180 °F |
|
Ascend Performance Materials VYDYNE® R400G Nylon, Mineral and Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermocomp® FP-VC-1003 BK8-019 Polyvinylidene Fluoride, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry) Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering .. |
|||
CTE, linear | 31.0 - 50.4 µm/m-°C | 17.2 - 28.0 µin/in-°F | Average value: 37.4 µm/m-°C Grade Count:9 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
CTE, linear | 31.0 - 53.0 µm/m-°C | 17.2 - 29.4 µin/in-°F | Average value: 41.3 µm/m-°C Grade Count:7 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
CTE, linear | 31.0 µm/m-°C @Temperature 20.0 °C |
17.2 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermotuf® QF-1006 HI Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |