Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.00 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
2.22 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP545 Carbon Fiber
(discontinued **) Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high .. |
|||
CTE, linear | 4.00 - 95.1 µm/m-°C | 2.22 - 52.8 µin/in-°F | Average value: 55.2 µm/m-°C Grade Count:26 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
CTE, linear | 4.00 µm/m-°C | 2.22 µin/in-°F | ISO 11359-2 |
Celanese VECTRA A950 LCP
(Unverified Data**) Unreinforced Vectra grade suitable for extrusion. suitable for extrusionA three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed fligh.. |
|||
CTE, linear | 4.00 µm/m-°C | 2.22 µin/in-°F | ISO 11359-2 |
Celanese VECTRA MT1300 LCP, Medical Technology
(Unverified Data**) Unreinforced Vectra grade suitable for extrusion. suitable for extrusionA three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flight.. |
|||
CTE, linear | 4.00 µm/m-°C | 2.22 µin/in-°F | ISO 11359-2 |
Celanese ZENITE 6140L LCP, 40% Glass Reinforced
(Unverified Data**) Zenite® 6140L is a 40% glass fiber reinforced and lubricated liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.40% glass rei.. |
|||
CTE, linear | 4.00 - 12.0 µm/m-°C | 2.22 - 6.67 µin/in-°F | |
MarkeTech Gadolinium silicate:Cerium (GSO:Ce; Gd2SiO5) Scintillator Crystal Gadolinium silicate doped with cerium is a "fast" crystal and can be used as a protection scintillator. Its possible applications include computer tomography, spatial resolution of less than 1 mm. I.. |
|||
CTE, linear | 4.00 - 11.0 µm/m-°C | 2.22 - 6.11 µin/in-°F | |
MarkeTech Yttrium aluminum perovskite:Cerium (YAP:Ce; YAlO3) Scintillator Crystal Yttrium aluminum perovskite activated by cerium is a fast, mechanically strong and chemically resistant scintillation material. Mechanical properties enable precise machining and entrance windows ca.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -50.0 - 50.0 °C |
2.22 µin/in-°F @Temperature -58.0 - 122 °F |
|
Mateck Fused Silica UV-VIS Grade (SiO2) Optical crystals |
|||
CTE, linear | 4.00 - 6.00 µm/m-°C @Temperature 20.0 °C |
2.22 - 3.33 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials AC6043 Titanium Diboride/Boron Nitride Composite TiB2/BN. Density is 83-92% of theoretical. Sonic Modular1 is 4 to 17 x 10^6 psi.Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other r.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 25.0 - 1500 °C |
2.22 µin/in-°F @Temperature 77.0 - 2730 °F |
Parallel to pressing direction |
Momentive Performance Materials HBN Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 25.0 - 1500 °C |
2.22 µin/in-°F @Temperature 77.0 - 2730 °F |
Parallel to pressing direction |
Momentive Performance Materials HBR Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GM27884 Dental Glass Remarks: Ba-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott GM32087 Dental Glass Remarks: Sr-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NanoFine 180 Dental Glass NanoFine 180 falls between UltraFine powders and the common nano powders, this grain size can open up new dimensions of filler load, transparency and polishability.AdvantagesFirst refractive index m.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
UBE Tyranno Grade ZMI Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C | 2.22 - 2.78 µin/in-°F | |
Master Bond EP17HT-3 One component, snap-curing epoxy system Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 20.0 - 400 °C |
2.22 µin/in-°F @Temperature 68.0 - 752 °F |
|
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 20.0 - 400 °C |
2.22 µin/in-°F @Temperature 68.0 - 752 °F |
|
Zircar Refractory Composites RS-99-60 Refractory Sheet ZRCI Refractory Sheet Type RS-99-60 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BPR-DS Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BTN-2 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories COD-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 1000 °C |
2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CRAG-S50 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-669 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-738 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-804 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature 1000 °C |
2.22 - 2.78 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-810 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.00 - 5.00 µm/m-°C @Temperature <=1000 °C |
2.22 - 2.78 µin/in-°F @Temperature <=1830 °F |
|
Acerde Silicon Carbide Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert.. |
|||
CTE, linear | 4.00 µm/m-°C @Temperature 20.0 °C |
2.22 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Celanese VECTRA® H140 40% Glass Filled Liquid Crystal Polymer (LCP) Description: An easily processable LCP with the highest temperature capability 40% glass filledInformation provided by Celanese Corporation. |
|||
CTE, linear | 4.00 µm/m-°C | 2.22 µin/in-°F | In Plane; ASTM E289-95 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |
|||
CTE, linear | 4.00 - 500 µm/m-°C @Temperature 55.0 - 160 °C |
2.22 - 278 µin/in-°F @Temperature 131 - 320 °F |
Average value: 376 µm/m-°C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |