Gwent Electronic Materials C2020322D6 Platinum Polymeric Ink

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2020322D6 Platinum Polymeric Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C2020322D6 is a screen printable Platinum ink designed for printing working electrodes in electrochemical sensor applications. The paste can be used to detect H2O2, is suitable for developing biosensors with oxidase enzymes, DNA or immune-sensors. The ink is designed for curing on polymer substrates, has excellent chemical and environmental resistance, and is suitable for fine line printing. Screen Printing Equipment: semi-automatic, automaticScreen Types: stainless steel, polyester, mesh 156-325tpiSubstrate: polyester, PVC, polycarbonate or ceramicInformation provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 85.5 - 86.5 %

@Temperature 700 °C
85.5 - 86.5 %

@Temperature 1290 °F
Viscosity 10000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
10000 - 15000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.29 ohm
0.29 ohm
Normalized to 25 microns
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 130 °C
0.0500 hour

@Temperature 266 °F
belt dryer
30.0 min

@Temperature 180 °C
0.500 hour

@Temperature 356 °F
60.0 min

@Temperature 130 °C
1.00 hour

@Temperature 266 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 95.4
Using a 230 mesh stainless steel screen