Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0100 - 1.00e+16 ohm-cm | 0.0100 - 1.00e+16 ohm-cm | Average value: 2.76e+15 ohm-cm Grade Count:79 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Electrical Resistivity | 10.0 - 1.00e+16 ohm-cm | 10.0 - 1.00e+16 ohm-cm | Average value: 2.97e+14 ohm-cm Grade Count:20 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 2.18e+15 ohm-cm Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 3.25e+15 ohm-cm Grade Count:4 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Electrical Resistivity | 10000 - 1.00e+16 ohm-cm | 10000 - 1.00e+16 ohm-cm | Average value: 1.10e+15 ohm-cm Grade Count:33 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.51e+15 ohm-cm Grade Count:7 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+16 ohm-cm | 1.00e+11 - 1.00e+16 ohm-cm | Average value: 1.38e+15 ohm-cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 2.60e+15 ohm-cm Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Electrical Resistivity | 500000 - 1.00e+16 ohm-cm | 500000 - 1.00e+16 ohm-cm | Average value: 2.88e+15 ohm-cm Grade Count:33 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 7.75e+15 ohm-cm Grade Count:4 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.42e+15 ohm-cm Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Electrical Resistivity | 1000 - 1.00e+16 ohm-cm | 1000 - 1.00e+16 ohm-cm | Average value: 6.64e+15 ohm-cm Grade Count:22 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 8.71e+15 ohm-cm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 8.66e+14 ohm-cm Grade Count:24 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Electrical Resistivity | 1.00e+9 - 1.00e+16 ohm-cm | 1.00e+9 - 1.00e+16 ohm-cm | Average value: 4.47e+14 ohm-cm Grade Count:24 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Electrical Resistivity | 460 - 1.00e+16 ohm-cm | 460 - 1.00e+16 ohm-cm | Average value: 8.77e+14 ohm-cm Grade Count:31 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 2.46e+14 ohm-cm Grade Count:270 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 2.29e+15 ohm-cm Grade Count:14 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.56e+15 ohm-cm Grade Count:17 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 1.09e+15 ohm-cm Grade Count:10 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 5.88e+15 ohm-cm Grade Count:19 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 2.68e+15 ohm-cm Grade Count:12 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | |
3M Dyneon™ Aflas® FA-100H PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Electrical Resistivity | 1.00e+12 - 1.00e+16 ohm-cm | 1.00e+12 - 1.00e+16 ohm-cm | Average value: 1.48e+15 ohm-cm Grade Count:15 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | Average value: 8.11e+15 ohm-cm Grade Count:38 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00e+14 - 1.00e+16 ohm-cm | 1.00e+14 - 1.00e+16 ohm-cm | Average value: 9.65e+14 ohm-cm Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 4.00e+14 - 1.00e+16 ohm-cm | 4.00e+14 - 1.00e+16 ohm-cm | Average value: 5.43e+15 ohm-cm Grade Count:7 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 100 - 1.00e+16 ohm-cm | 100 - 1.00e+16 ohm-cm | Average value: 5.17e+15 ohm-cm Grade Count:6 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Electrical Resistivity | 1.00e+15 - 1.00e+16 ohm-cm | 1.00e+15 - 1.00e+16 ohm-cm | |
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |