Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific) Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific) Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
PLC 0; UL 746 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
BK |
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
(dis Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | Average value: 5.00 mm/min Grade Count:5 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
(BK) |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.50 mm |
0.000 - 0.394 in/min @Thickness 0.0591 in |
BK |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL746A |
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL746A |
Idemitsu Kosan Xarec® WA 552 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled/Impact Modified. Used in Automotive and Industrial applications. NSF and medical approval ISO 10993 |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Asia Pacific) Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.57 mm |
0.000 - 0.394 in/min @Thickness 0.0618 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 1.47 mm |
0.000 - 0.394 in/min @Thickness 0.0579 in |
UL PLC 0 (0-10 mm/min) |
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746A |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
UL PLC 0 (0-10 mm/min) |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.05 mm |
0.000 - 0.394 in/min @Thickness 0.120 in |
UL PLC 0 (0-10 mm/min) |
Resinoid 1322 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
BK |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 3.00 mm |
0.000 - 0.394 in/min @Thickness 0.118 in |
BK |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min | 0.000 - 0.394 in/min | UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 0.000 - 10.0 mm/min @Thickness 6.10 mm |
0.000 - 0.394 in/min @Thickness 0.240 in |
UL PLC 0 (0-10 mm/min) |
Resinoid 7201 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |