Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AK Steel ASTM A 607 Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA)

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer AK Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AK Steel ASTM A 607 Class 2 Formable, Grade 60K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. AK Steel Formable Grade - K indicates killed.Information provided by AK Steel
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 480 MPa
>= 69600 psi
Tensile Strength, Yield >= 410 MPa
>= 59500 psi
Elongation at Break >= 18 %
>= 18 %
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 12.4 µm/m-°C

@Temperature 20.0 - 100 °C
6.89 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 50.0 - 100 °C
0.115 BTU/lb-°F

@Temperature 122 - 212 °F
Thermal Conductivity 89.0 W/m-K
618 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000142 ohm-cm
0.0000142 ohm-cm