Material Notes:
AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a combination of high elongation and electric properties.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
Part B
1.17 g/cc
0.0424 lb/in³
Part A
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.58 MPa
1100 psi
Elongation at Break 140 %
140 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air <= 25.0 °C
<= 77.0 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
Dielectric Constant 4.2

@Frequency 60.0 Hz,
Temperature 23.0 °C
4.2

@Frequency 60.0 Hz,
Temperature 73.4 °F
4.3

@Frequency 60.0 Hz,
Temperature 150 °C
4.3

@Frequency 60.0 Hz,
Temperature 302 °F
4.9

@Frequency 60.0 Hz,
Temperature 100 °C
4.9

@Frequency 60.0 Hz,
Temperature 212 °F
Dissipation Factor 0.030

@Frequency 60.0 Hz,
Temperature 23.0 °C
0.030

@Frequency 60.0 Hz,
Temperature 73.4 °F
0.040

@Frequency 60.0 Hz,
Temperature 100 °C
0.040

@Frequency 60.0 Hz,
Temperature 212 °F
0.040

@Frequency 60.0 Hz,
Temperature 150 °C
0.040

@Frequency 60.0 Hz,
Temperature 302 °F
Arc Resistance >= 150 sec
>= 150 sec
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 100 °C
2.00 - 3.00 hour

@Temperature 212 °F
60.0 - 240 min

@Temperature 120 - 160 °C
1.00 - 4.00 hour

@Temperature 248 - 320 °F
optional
Pot Life 30 min

@Temperature 80.0 °C
30 min

@Temperature 176 °F
>= 480 min

@Temperature 25.0 °C
>= 480 min

@Temperature 77.0 °F
Descriptive Properties Value Comments
Arc-Track Free (min) > 1500
2.5 KV
Color Clear
Parts by Weight (pbw) 100
Part A
112
Part B
Thermal Shock Resistance Scale 0 (poor) to 10 (excellent)