Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinforced polyester compound is suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, Corelyn can be supplied in logs, slugs, or bulk.Typical applications are microwave dishware and serving trays.
Physical Properties Metric English Comments
Specific Gravity 1.80 - 2.00 g/cc
1.80 - 2.00 g/cc
Water Absorption 0.20 - 0.40 %
0.20 - 0.40 %
24 hours, 23°C
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 60 - 70
60 - 70
Tensile Strength, Ultimate 27.6 - 48.3 MPa
4000 - 7000 psi
Flexural Strength 82.7 - 110 MPa
12000 - 16000 psi
Flexural Modulus 11.7 - 14.5 GPa
1700 - 2100 ksi
Compressive Strength 110 - 138 MPa
16000 - 20000 psi
Izod Impact, Notched 1.07 - 2.67 J/cm
2.00 - 5.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Mold Temperature 160 - 182 °C
320 - 360 °F