CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer CTC (Composite Technologies)
Trade Name X-PRO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC).
Physical Properties Metric English Comments
Melt Flow 20 g/10 min
20 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ISO 527-1/2
Flexural Modulus 0.862 GPa
125 ksi
0.05 in/min; ISO 178
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ISO 180/A
Processing Properties Metric English Comments
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
Middle Barrel Temperature 193 - 227 °C
380 - 440 °F
Front Barrel Temperature 204 - 216 °C
400 - 420 °F
Nozzle Temperature 204 - 216 °C
400 - 420 °F
Melt Temperature 204 - 227 °C
400 - 440 °F
Mold Temperature 26.7 - 60.0 °C
80.0 - 140 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 150 psi
Clamp Pressure 27.6 - 34.5 MPa
4000 - 5000 psi
Descriptive Properties Value Comments
Boost Pressure (psi) 500-1500
Color General Purpose Black
Hold Pressure 50 - 75% of Boost
Screw Speed Medium to Fast