Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound

Category Ceramic , Polymer , Thermoset , Epoxy
Manufacturer Chesterton
Trade Name ARC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a thickness of 3 mm (1/8”) or more. Non-shrinking. 100% Solids. ARC MX5 is formulated with a high concentration of small ceramic beads and particles for extremely abrasive environments where metal loss is often repaired by more conventional and costly weld overlay. ARC MX5 can be used either to rebuild eroded metal surfaces or to provide a wear resistant, sacrificial surface which frequently outperforms the original metal, rubber liners, ceramic tiles or weld overlay. ARC MX5 is chosen over other ARC Composites for abrasion when a rapid cure, emergency repair is needed.Benefits:Excellent wear characteristics of ARC MX5 extend equipment operating cycles.Tough resin structures resist thermal-mechanical shockOutstanding adhesion results in reliable performance with no undercuttingEase of application reduces labor and downtime costsRapid cure allow return to service in 1 hour or less.Easily shaped and formed to any metal surface. Suggested Uses:Pneumatic ConveyorsChipper and Chip BinsHydro PulpersTurbo SeparatorsNi-Hard Slurry PumpsFly Ash SeparatorsWood Chip Transport FansScrew ConveyorsExhaust FansCyclones, HoppersWear PlatesPipe ElbowsPulverized Fuel LinesPulverizers Information provided by Chesterton
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Cured
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength at Break 16.5 MPa
2400 psi
ASTM D638
Flexural Strength 24.1 MPa
3500 psi
ASTM D790
Compressive Strength 63.4 MPa
9200 psi
ASTM D695
Impact Test 6.55 J
4.83 ft-lb
Reverse; ASTM D2794
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Wet Service
120 °C
248 °F
Dry Service
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 43.0 °C
0.0830 hour

@Temperature 109 °F
Tack Free
10.0 min

@Temperature 32.0 °C
0.167 hour

@Temperature 89.6 °F
Tack Free
10.0 min

@Temperature 43.0 °C
0.167 hour

@Temperature 109 °F
Light Load
15.0 min

@Temperature 25.0 °C
0.250 hour

@Temperature 77.0 °F
Tack Free
19.8 min

@Temperature 32.0 °C
0.330 hour

@Temperature 89.6 °F
Light Load
25.00 min

@Temperature 16.0 °C
0.4167 hour

@Temperature 60.8 °F
Tack Free
30.0 min

@Temperature 25.0 °C
0.500 hour

@Temperature 77.0 °F
Light Load
30.0 min

@Temperature 43.0 °C
0.500 hour

@Temperature 109 °F
Full Load
35.0 min

@Temperature 10.0 °C
0.583 hour

@Temperature 50.0 °F
Tack Free
45.0 min

@Temperature 32.0 °C
0.750 hour

@Temperature 89.6 °F
Full Load
60.0 min

@Temperature 16.0 °C
1.00 hour

@Temperature 60.8 °F
Light Load
60.0 min

@Temperature 25.0 °C
1.00 hour

@Temperature 77.0 °F
Full Load
120 min

@Temperature 10.0 °C
2.00 hour

@Temperature 50.0 °F
Light Load
120 min

@Temperature 16.0 °C
2.00 hour

@Temperature 60.8 °F
Full Load
240 min

@Temperature 10.0 °C
4.00 hour

@Temperature 50.0 °F
Full Load
720 min

@Temperature 43.0 °C
12.0 hour

@Temperature 109 °F
Full Chemical
1080 min

@Temperature 32.0 °C
18.0 hour

@Temperature 89.6 °F
Full Chemical
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Full Chemical
2160 min

@Temperature 16.0 °C
36.0 hour

@Temperature 60.8 °F
Full Chemical
2880 min

@Temperature 10.0 °C
48.0 hour

@Temperature 50.0 °F
Full Chemical
Descriptive Properties Value Comments
Color Gray