Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break >= 150 %
>= 150 %
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 6.94 J/cm

@Temperature 22.8 °C
13.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 - 282 °C
490 - 540 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Dry Time 2 - 4 hour

@Temperature 121 °C
2 - 4 hour

@Temperature 250 °F
to ensure the moisture level is less than 0.02%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm