Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 40% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shrinkageHigh heat distortion temperatureLow moisture absorptionResistant to boiling waterHigh creep resistance Application examples:Functional parts in hot waterValves in beverage dispensersInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Water Absorption 1.5 %
1.5 %
ISO 62
Moisture Absorption 0.800 %
0.800 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 160 MPa
23200 psi
conditioned; ISO 2039-1
Tensile Strength at Break 130 MPa
18900 psi
conditioned; ISO 527-1/-2
140 MPa
20300 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
2.0 %
2.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 9.00 GPa
1310 ksi
conditioned; ISO 527-1/-2
9.00 GPa
1310 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
conditioned; ISO 179/1eU
4.50 J/cm²

@Temperature 30.0 °C
21.4 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
conditioned; ISO 179/1eA
1.30 J/cm²

@Temperature 30.0 °C
6.19 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
125 °C
257 °F
short term; EMS
Transformation Temperature, Tg 155 °C
311 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Cooling and climate control
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Electrical equipment
Energy distribution
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Heating systems
Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Tools & Accessories
Processing Injection Molding
Water Contact NSF 61
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved