Humiseal 1A20LSE Urethane Conformal Coating

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Humiseal
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Humiseal 1A20LSE Urethane Conformal Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses thermal shock test (MIL-I-46058C)Flammability (self extinguishing) (ASTM D635)Excellent resistance to solvents (IPC CC 830)Recommended Stripper: 1071Recommended Thinner: 801 Cure Type: Room Temp or Heat
Physical Properties Metric English Comments
Density 0.899 g/cc
0.0325 lb/in³
ASTM D1475
Solids Content 50 %
50 %
Fed Std 141 Method 4044
Volatile Organic Compounds (VOC) Content <= 225 g/l
<= 225 g/l
Viscosity 100 cP
100 cP
Fed Std Method 4287
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.089590 GPa
12.994 ksi
Thermal Properties Metric English Comments
CTE, linear 510 µm/m-°C

@Temperature 20.0 °C
283 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Glass Transition Temp, Tg 71.0 °C
160 °F
Flash Point 15.6 °C
60.0 °F
ASTM D56
Electrical Properties Metric English Comments
Surface Resistance 4.80e+10 ohm
4.80e+10 ohm
Moisture Resistance; MIL-I-46058C
Insulation Resistance 3.00e+14 ohm
3.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Dielectric Constant 3.5
3.5
ASTM D1 50 65T
Dielectric Breakdown >= 1500 V
>= 1500 V
Dielectric Withstand; MIL-I-46058C
Dissipation Factor 0.028
0.028
ASTM D1 50 65T
Processing Properties Metric English Comments
Cure Time 20.0 min
0.333 hour
Dry Time to Handling; Fed Std 141 4061
30.0 min

@Temperature 170 °C
0.500 hour

@Temperature 338 °F
>= 1440 min

@Temperature 23.0 °C
>= 24.0 hour

@Temperature 73.4 °F
Shelf Life 6.00 Month

@Temperature 23.0 °C
6.00 Month

@Temperature 73.4 °F
Descriptive Properties Value Comments
Coverage 375 ft²/gal