Afton is a fine-grained kaolin used asa a filler in hard rubber products, plastic products, adhesives, protective coatings and similar applications.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 72 %
72 %
G.E. Brightness
Oil Absorption 41 %
41 %
g/100g clay; ASTM D-281
Particle Size 0.30 µm
0.30 µm
median
0.50 µm
0.50 µm
71.5% finer than
1.0 µm
1.0 µm
86% finer than
2.0 µm
2.0 µm
92% finer than
5.0 µm
5.0 µm
98% finer than
10 µm
10 µm
98.5% finer than
20 µm
20 µm
99.5% finer than
Particle Mesh Size 325 Mesh
325 Mesh
0.5% retained
pH 4.0
4.0
10% solids
Specific Surface Area 22 - 24 m²/g
22 - 24 m²/g
Component Elements Properties Metric English Comments
Al2O3 38.8 %
38.8 %
CaO 0.15 %
0.15 %
Fe2O3 1.2 %
1.2 %
K2O 0.20 %
0.20 %
Loss on Ignition(%) 14 %
14 %
MgO 0.060 %
0.060 %
Na2O 0.15 %
0.15 %
SiO2 44 %
44 %
TiO2 1.46 %
1.46 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %