Material Notes:
Middle viscosity, BLACKApplications A variety of reservoir tanks and housingsInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Moisture Absorption at Equilibrium 1.3 %
1.3 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 123 MPa
17800 psi
ASTM D790
Flexural Modulus 2.746 GPa
398.3 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C
38.9 µin/in-°F
ASTM D696
Melting Point 255 °C
491 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Dielectric Constant 3.3
3.3
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Arc Resistance 128 sec
128 sec
ASTM D495