Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latishield 73/13-07A POM, Steel Fiber Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Steel Filled
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 73/13-07A POM, Steel Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Linear Mold Shrinkage, Flow 0.020 - 0.023 cm/cm
0.020 - 0.023 in/in
Linear Mold Shrinkage, Transverse 0.0205 - 0.0225 cm/cm
0.0205 - 0.0225 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
Elongation at Break 20 %
20 %
Elongation at Yield 8.5 %
8.5 %
Tensile Modulus 3.00 GPa
435 ksi
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Vicat Softening Point 150 °C

@Load 5.00 kg
302 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 135 ohm-cm
135 ohm-cm
Surface Resistance 48 ohm
48 ohm
Processing Properties Metric English Comments
Melt Temperature 175 - 200 °C
347 - 392 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Descriptive Properties Value Comments
Electromagnetic reflection 95 dB
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: