Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 175 - 220 °C | 347 - 428 °F | |
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
DuPont Nucrel® 1302 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
(discontinued **) 13 wt% Methacrylic Acid.Nucrel® 1302 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process po.. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 195 °C Grade Count:22 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Melt Temperature | 175 - 238 °C | 347 - 460 °F | Degrades above 238°C. |
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly.. |
|||
Melt Temperature | 175 - 190 °C | 347 - 374 °F | |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 13 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 13E71 POM Polyoxymethylene (POM). Toughened. Medium viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided .. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 2 POM Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 23UVE71 POM Polyoxymethylene (POM). UV stabilized. Toughened. Low viscosity. Good elongation and impact resistance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 3E71 POM Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latan 9 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13-01M POM, Molybdenum disulphide Filled Self-lubricating product based on Polyoxymethylene (POM). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13-20T POM, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latistat 73/13-06 POM Dissipative product based on Polyoxymethylene (POM). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Melt Temperature | 175 - 230 °C | 347 - 446 °F | Extrusion Coating |
DuPont™ Elvax® 3155 Ethylene Vinyl Acetate DuPont™ Elvax® 3155 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 31.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | Extrusion Coating |
DuPont™ Elvax® 3175LGA Ethylene Vinyl Acetate DuPont™ Elvax® 3175LGA is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Melt Temperature | 175 - 230 °C | 347 - 446 °F | Extrusion Coating |
DuPont™ Elvax® 3178Z Ethylene Vinyl Acetate DuPont™ Elvax® 3178Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Melt Temperature | 175 °C | 347 °F | |
AdvanSource Biomaterials HYDROTHANE™ Hydrophilic Thermoplastic Polyurethane AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether aliphatic polyurethanes designed for use as coatings of catheters, sutures, intr.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
Huntsman Rexell® V8402 Cast Film Extrusion LLDPE
(discontinued **) Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent mechanical strength, low sealing temperature, and good flex crack resistanceApplications: Sealing layer in.. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 194 °C Grade Count:62 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 175 - 218 °C | 347 - 425 °F | Average value: 198 °C Grade Count:27 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 185 °C | 347 - 365 °F | |
Huntsman PE1335 EVA Film Extrusion
(discontinued **) 3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Melt Temperature | 175 - 215 °C | 347 - 419 °F | |
DuPont Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melt Temperature | 175 - 200 °C | 347 - 392 °F | |
LATI Latilub 73/13 Y/20 POM, 20% Aramid Fiber Reinforced Self-lubricating product based on Polyoxymethylene (POM). Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |