Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Electrically Conductive
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated temperatures. The conductive bonds are remarkably adaptable to thermal cycling and resistant to chemicals including water and oil, over the exceptionally wide temperature range of 4 K to +275°F, enabling it to be serviceable even in cryogenic applications.
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 5.52 MPa
>= 800 psi
After 30 days water immersion
>= 5.86 MPa

@Temperature 23.0 °C
>= 850 psi

@Temperature 73.4 °F
Peel Strength >= 1.75 kN/m
>= 10.0 pli
Thermal Properties Metric English Comments
Thermal Conductivity 1.30 W/m-K
9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -269 °C
-452 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
1440 - 2880 min

@Temperature 23.9 °C
24.0 - 48.0 hour

@Temperature 75.0 °F
Pot Life 45 - 60 min
45 - 60 min
100 gm mass
Shelf Life 3.00 Month
3.00 Month
syringe
6.00 Month
6.00 Month
glass jar
Descriptive Properties Value Comments
Mixing Ratio (A to B) 1/1
Viscosity smooth paste
Users viewing this material also viewed the following: