Parker Chomerics Tecknit Teckfip™ FIP-N (LD) Formed in Place Conductive Elastomer

Category Polymer
Manufacturer Parker Chomerics Tecknit
Trade Name Teckfip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit Teckfip™ FIP-N (LD) Formed in Place Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: FIP-N is similar in performance to FIP-A elastomer and hence offers a good non-corrosive EMI shield in harsh conditions. This material is one of our more cost effective FIP compoundsInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 2.975 - 4.025 g/cc
2.975 - 4.025 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 41 - 55
41 - 55
Tensile Strength >= 1.38 MPa
>= 200 psi
Elongation at Break >= 50 %
>= 50 %
Peel Strength >= 9.00 kN/m
>= 51.4 pli
Compression Set 10 - 25 %
10 - 25 %
28 %

@Temperature 70.0 °C,
Time 79200 sec
28 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.020 ohm-cm
<= 0.020 ohm-cm
Surface Resistance <= 0.020 ohm
<= 0.020 ohm
Processing Properties Metric English Comments
Dry Time >= 0.200 hour
>= 0.200 hour
Tack Free
Cure Time <= 1440 min
<= 24.0 hour
Shelf Life 1.00 Month
1.00 Month
Syringe
6.00 Month
6.00 Month
Cartridge
Descriptive Properties Value Comments
Color Pale Yellow
Filler Silver/Nickel