Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 60% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby tools, gears, covers of electric appliances, cooling skrews of blowers, electromotors, carrying parts in the automotive industry. Replacement of metal parts from ZAMAC and etc.Delivered in natural mode and in black.Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 270 MPa
39200 psi
Elongation at Break 2.3 %
2.3 %
Tensile Modulus 22.8 GPa
3310 ksi
Flexural Strength 420 MPa
60900 psi
Flexural Modulus 18.3 GPa
2650 ksi
Charpy Impact Unnotched 9.50 J/cm²

@Temperature -20.0 °C
45.2 ft-lb/in²

@Temperature -4.00 °F
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.80 J/cm²

@Temperature -20.0 °C
8.57 ft-lb/in²

@Temperature -4.00 °F
2.60 J/cm²

@Temperature 23.0 °C
12.4 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
Deflection Temperature at 1.8 MPa (264 psi) 218 °C
424 °F
Vicat Softening Point 222 °C
432 °F
Flammability Test 1.0
1.0
Glow Wire Test 650 °C
1200 °F
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+12 ohm-cm
6.00e+12 ohm-cm
Dielectric Strength 33.0 kV/mm
838 kV/in
Comparative Tracking Index 600 V
600 V
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 90.0 - 100 °C
194 - 212 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 4 hour
4 hour
Moisture Content 0.10 %
0.10 %
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi
Users viewing this material also viewed the following: