Polimeri Europa Eraclene® MP 94 U High Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Eraclene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Eraclene® MP 94 U High Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eraclene MP 94 U is a gas phase high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a high density that make it ideal for injection molding applications where outstanding rigidity, warp resistance and toughness are required. The polymer has high thermal stability during extrusion. This grade is UV stabilized and it is suitable for the production of items for outdoor exposure.Main Applications: Eraclene MP 94 U is an injection molding grade designed for molded crates, cases, toys, trays and other similar objects requiring rigidity.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ISO 1183
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
21 g/10 min

@Load 5.00 kg,
Temperature 190 °C
21 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ISO 868/A
Tensile Strength at Break 17.0 MPa
2470 psi
ISO 527
Tensile Strength, Yield 30.0 MPa
4350 psi
ISO 527
Elongation at Break 400 %
400 %
ISO 527
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ISO 180/A
Thermal Properties Metric English Comments
Melting Point 137 °C
279 °F
Internal method
Vicat Softening Point 128 °C

@Load 1.00 kg
262 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746