Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Flexirene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characterized by a good rigidity and an optimum processability.Main Applications: Flexirene FH 56 A is recommended for the production of general purpose film in blend or in coextrusion with LDPE. It is also used for the production of nets because of its perfect balance between rigidity and processability.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.934 g/cc
0.934 g/cc
ISO 1183
Thickness 15.0 - 50.0 microns
0.591 - 1.97 mil
Recommended
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 16.0 MPa
2320 psi
ISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPa
2610 psi
ISO 527-3
Film Elongation at Break, MD 650 %
650 %
ISO 527-3
Film Elongation at Break, TD 800 %
800 %
ISO 527-3
Coefficient of Friction, Dynamic >= 0.50
>= 0.50
ISO 8295
Elmendorf Tear Strength, MD 0.7133 g/micron
18.12 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 6.114 g/micron
155.3 g/mil
ISO 6383-2
Dart Drop Test 55.0 g
0.121 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ISO 527-3
Film Tensile Strength at Break, TD 32.0 MPa
4640 psi
ISO 527-3
1% Secant Modulus, MD 390 MPa
56600 psi
ISO 527-3
1% Secant Modulus, TD 450 MPa
65300 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
Internal method
Vicat Softening Point 117 °C

@Load 1.00 kg
243 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 14 %
14 %
ISO 14782
Gloss 50 %
50 %
45°; ASTM D2457