Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Nylatron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybdenum disulphide results in an improved crystalline structure enhancing bearing and wear properties. High mechanical strength, stiffness, hardness and toughness Good fatigue resistance High mechanical damping ability Good sliding properties Excellent wear resistance Good electrical insulating properties Good resistance to high energy radiation (gamma- and X-rays) Good machinability
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH
Water Absorption at Saturation 7.8 %
7.8 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
ISO 2039-2
Hardness, Shore D 80
80
Ball Indentation Hardness 165 MPa
23900 psi
ISO 2039-1
Tensile Strength 95.0 MPa
13800 psi
at Yield; ISO 527-1/-2
Elongation at Break 20 %
20 %
ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 3.60 GPa
522 ksi
ISO 527-1/-2
Flexural Strength 128 MPa
18600 psi
Flexural Modulus 3.24 GPa
470 ksi
Compressive Strength 32.0 MPa

@Strain 1 %
4640 psi

@Strain 1 %
ISO 604
62.0 MPa

@Strain 2 %
8990 psi

@Strain 2 %
ISO 604
100 MPa

@Strain 5 %
14500 psi

@Strain 5 %
ISO 604
K Factor (ISO) 12 µm/km
12 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35 - 0.55
0.35 - 0.55
Limiting Pressure Velocity 0.0800 MPa-m/sec
2280 psi-ft/min
at 1 m/s unlubricated
0.130 MPa-m/sec
3710 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
Melting Point 260 °C
500 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous; 20,000 h
95.0 °C
203 °F
Continuous; 5,000 h
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index 26 %
26 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency >=100000 Hz
3.8

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
Dissipation Factor 0.013

@Frequency 100000 Hz
0.013

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Limited
Limited
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Users viewing this material also viewed the following: