SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DL0029E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
5 mm/min; ISO 527
Elongation at Yield 5.1 %
5.1 %
5 mm/min; ISO 527
Tensile Modulus 2.40 GPa
348 ksi
1 mm/min; ISO 527
Flexural Yield Strength 88.0 MPa
12800 psi
2 mm/min; ISO 178
Flexural Modulus 2.20 GPa
319 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 135 kJ/m²
64.2 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 75.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
41.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 72.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
40.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 139 °C
282 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in
UL 94