| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.64 g/cc | 0.0592 lb/in³ | ASTM D792 | 
| Apparent Bulk Density | 0.270 g/cc | 0.00975 lb/in³ | |
| Water Absorption | 0.35 % | 0.35 % | 48 hours, 50°C. ASTM D570 | 
| Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Compression Molding. ASTM D955 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 | 
| Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 | 
| Flexural Modulus | 13.8 GPa | 2000 ksi | ASTM D790 | 
| Compressive Yield Strength | 152 MPa | 22000 psi | ASTM D695 | 
| Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | ASTM D256A | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow |           18.0           µm/m-°C           @Temperature 20.0 °C  | 
                  10.0           µin/in-°F           @Temperature 68.0 °F  | 
        ASTM D696 | 
| Thermal Conductivity | 0.322 W/m-K | 2.23 BTU-in/hr-ft²-°F | ASTM F433 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 260 °C | 500 °F | ASTM D648A | 
| Oxygen Index | 29 % | 29 % | ASTM D2863 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Dielectric Constant |           4.0                     @Frequency 1e+6 Hz  | 
                  4.0                     @Frequency 1e+6 Hz  | 
        Wet | 
|           4.2                     @Frequency 1000 Hz  | 
                  4.2                     @Frequency 1000 Hz  | 
        Wet | |
| Dielectric Strength | 14.0 kV/mm | 356 kV/in | Wet, step-by-step. ASTM D149 | 
| 15.0 kV/mm | 381 kV/in | Wet, short term. ASTM D149 | |
| Dissipation Factor |           0.010                     @Frequency 1000 Hz  | 
                  0.010                     @Frequency 1000 Hz  | 
        Wet; ASTM D150 | 
|           0.014                     @Frequency 1e+6 Hz  | 
                  0.014                     @Frequency 1e+6 Hz  | 
        Wet; ASTM D150 | |
| Arc Resistance | 138 sec | 138 sec | ASTM D495 | 
| Comparative Tracking Index | >= 600 V | >= 600 V | UL746A, ASTM D3638 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Processing Temperature | 160 - 180 °C | 320 - 356 °F | Mold temperature |