Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6 GF50 LE 50% Glass Filled (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.75 %

@Time 86400 sec
0.75 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 cm/cm

@Thickness 3.17 mm
0.0025 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 193 MPa
28000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 269 MPa
39000 psi
ASTM D790
Flexural Modulus 10.7 GPa
1550 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256