Tipco Tipcolene® FPDG-M FPDG M - 28% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolene® FPDG-M FPDG M - 28% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral Reinforced, High Stiffness, High Impact PP CompoundApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Flexural Modulus 2.65 GPa
384 ksi
ASTM D790
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648