Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy

Category Polymer , Thermoplastic
Manufacturer Wolf Kunststoff
Trade Name ZEDEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stress resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve TechnologyInformation provided by Zedex
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Water Absorption 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
RMC 93%; DIN EN ISO 62
Moisture Absorption at Equilibrium 0.50 %
0.50 %
DIN EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore A >= 100
>= 100
DIN 53505
Hardness, Shore D 85
85
DIN 53505
Ball Indentation Hardness 110 MPa
16000 psi
DIN 2039
Tensile Strength at Break 45.0 MPa
6530 psi
DIN EN ISO 527
Tensile Strength 45.0 MPa
6530 psi
DIN EN ISO 527
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
5080 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Tensile Strength, Yield 35.8 MPa
5190 psi
Elastic Limit
Elongation at Break 3.1 %
3.1 %
Flexural; DIN EN ISO 178
3.1 %
3.1 %
DIN EN ISO 527
Elongation at Yield 2.1 %
2.1 %
Elastic Yield Point
2.2 %
2.2 %
Flexural; DIN EN ISO 178
3.1 %
3.1 %
Elongation at Maximum Force; DIN EN ISO 527
Tensile Modulus 3.10 GPa
450 ksi
DIN EN ISO 527
Flexural Strength 68.0 MPa
9860 psi
DIN EN ISO 178
68.0 MPa
9860 psi
DIN EN ISO 178
103 MPa
14900 psi
Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178
Flexural Modulus 3.32 GPa
482 ksi
DIN EN ISO 178
Compressive Yield Strength 115 MPa
16700 psi
DIN EN ISO 604
Compressive Strength 95.0 MPa
13800 psi
Elastic Limit
112 MPa
16200 psi
break; DIN EN ISO 604
115 MPa
16700 psi
DIN EN ISO 604
48.0 MPa

@Time 3.60e+7 sec
6960 psi

@Time 10000 hour
86.0 MPa

@Time 360000 sec
12500 psi

@Time 100 hour
102 MPa

@Time 36.0 sec
14800 psi

@Time 0.0100 hour
19.0 MPa

@Strain 3.50 %
2760 psi

@Strain 3.50 %
DIN EN ISO 604
Compressive Modulus 4.011 GPa
581.7 ksi
DIN EN ISO 604
Fatigue Strength 35.0 MPa

@# of Cycles 1.00e+6
5080 psi

@# of Cycles 1.00e+6
1 Hz
K Factor (ISO) 0.40 µm/km

@Temperature 100 °C
0.40 µm/km

@Temperature 212 °F
0.50 µm/km

@Temperature 200 °C
0.50 µm/km

@Temperature 392 °F
0.50 µm/km

@Temperature 240 °C
0.50 µm/km

@Temperature 464 °F
1.5 µm/km

@Temperature 20.0 °C
1.5 µm/km

@Temperature 68.0 °F
Charpy Impact Unnotched NB
NB
EN ISO 179/1eU
Charpy Impact, Notched 2.47 J/cm²
11.8 ft-lb/in²
EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.17

@Temperature 20.0 °C
0.17

@Temperature 68.0 °F
Dry Operation
0.20

@Temperature 100 °C
0.20

@Temperature 212 °F
Dry Operation
Coefficient of Friction, Static 0.19

@Temperature 20.0 °C
0.19

@Temperature 68.0 °F
Dry Operation
Tensile Creep Modulus, 1000 hours 3200 MPa
464000 psi
At 1% Deformation; DIN 53444
Limiting Pressure Velocity 0.83333 MPa-m/sec
23792 psi-ft/min
v = 1m/min
2.50 MPa-m/sec
71400 psi-ft/min
v = 200m/min
2.567 MPa-m/sec
73280 psi-ft/min
v = 10m/min
3.90 MPa-m/sec
111000 psi-ft/min
v = 100m/min
Compression Set 6.0 %
6.0 %
Elastic Compression Limit
9.9 %
9.9 %
Nominal Compressive Yield Strain; DIN EN ISO 604
9.9 %
9.9 %
Nominal Compressive Strain at Compressive Strength; DIN EN ISO 604
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature <=100 °C
22.2 µin/in-°F

@Temperature <=212 °F
ISO E 830
47.0 µm/m-°C

@Temperature <=150 °C
26.1 µin/in-°F

@Temperature <=302 °F
ISO E 831
Specific Heat Capacity 1.18 J/g-°C
0.282 BTU/lb-°F
DSC
Melting Point 390 °C
734 °F
DSC
Maximum Service Temperature, Air 250 °C
482 °F
Pressed Bushings
280 °C
536 °F
Continuous
320 °C
608 °F
Short Term (3h)
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
DIN EN ISO 75
Glass Transition Temp, Tg 240 °C
464 °F
DSC
Flammability, UL94 V-0
V-0
Oxygen Index 52 %
52 %
DIN EN ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 93
Surface Resistance 5.00e+12 ohm
5.00e+12 ohm
IEC 93
Dielectric Constant 3.1

@Frequency 110 Hz
3.1

@Frequency 110 Hz
IEC 250
Dielectric Strength 21.0 kV/mm
533 kV/in
IEC 243
Dissipation Factor 0.00080
0.00080
IEC 112
0.078

@Frequency 1.00 Hz
0.078

@Frequency 1.00 Hz
Comparative Tracking Index 42 V
42 V
IEC 112
Descriptive Properties Value Comments
Alignment Adjustment 4
Nominal Scale: 1, low; 10, high
Chemical Sterilization 10
Nominal Scale: 1, low; 10, high
Color Ochre
Creep Resistance 3
Nominal Scale: 1, low; 10, high
Dimensional Stability with Thermal Expansion 9
Nominal Scale: 1, low; 10, high
Free from Silicon Applicable
Gamma-rays Radiation Sterilization 7
Nominal Scale: 1, low; 10, high
Machined Parts Applicable
Moist Heat Sterilization 6
Nominal Scale: 1, low; 10, high
Resistance Against dust, Dirt, Abrasive Substances 5
Nominal Scale: 1, low; 10, high
Resistance Against Hot Water 120
Resistance to Chemicals 5
Nominal Scale: 1, low; 10, high
Resistant Against Disinfectant Applicable
Rods up to Øe (de) Applicable
ROHS/WEEE Applicable
Sheets up to Maximum Thickness Applicable
Sliding Velocity 350
Suitable for Outdoor Use 9
Nominal Scale: 1, low; 10, high
Suitable for Vacuum Applicable
UV Rays Resistance 9
Nominal Scale: 1, low; 10, high