Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addiplast Addilene H 652 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Addiplast
Trade Name Addilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene H 652 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183/A
Melt Flow 28 g/10 min
28 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ISO 868
Tensile Strength at Break 33.0 MPa
4790 psi
ISO R 527
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO R 527
Elongation at Yield 10 %
10 %
ISO R 527
Modulus of Elasticity 1.35 GPa
196 ksi
ISO 178
Izod Impact, Notched (ISO) 2.50 kJ/m²
1.19 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/IeU
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-2/AF
Vicat Softening Point 150 °C
302 °F
ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
CEI 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A