| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adell DS-10 General Purpose Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Water Absorption | 0.25 % | 0.25 % | 24 hr immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
| Melt Flow | 9.0 - 11 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 - 11 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ASTM D785 |
| Tensile Strength, Ultimate | 69.0 MPa | 10000 psi | ASTM D638 |
| Elongation at Break | 130 % | 130 % | ASTM D638 |
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
| Flexural Modulus | 2.34 GPa | 339 ksi | ASTM D790 |
| Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm |
15.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |