| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET) |
| Manufacturer | BASF |
| Trade Name | Ultradur B |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
| Viscosity Test | 86 cm³/g | 86 cm³/g | Viscosity number |
| Melt Flow | 65 g/10 min @Load 2.16 kg, Temperature 275 °C |
65 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 110 MPa | 16000 psi | 5mm/min; ISO 527 |
| Elongation at Break | 1.9 % | 1.9 % | 5mm/min; ISO 527 |
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1mm/min; ISO 527 |
| Charpy Impact Unnotched | 2.60 J/cm² | 12.4 ft-lb/in² | ISO 179 |
| 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 | |
| Charpy Impact, Notched | 0.590 J/cm² | 2.81 ft-lb/in² | ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | 10 K/min |
| Deflection Temperature at 0.46 MPa (66 psi) | 214 °C | 417 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 180 °C | 356 °F | ISO 75 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | BK15029 | |
| Commercial Status | Active America | |
| Impact Modified | No | |
| Primary Processing Technique | Injection Molding |