BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
dry; ISO 1183
Water Absorption 7.2 %
7.2 %
beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
beginning dry (23°C/50% R.H.); ISO 62
Viscosity Test 140 cm³/g
140 cm³/g
Viscosity number
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.0 MPa
7980 psi
5mm/min; ISO 527
Elongation at Break 10 %
10 %
5mm/min; ISO 527
Tensile Modulus 4.20 GPa
609 ksi
1mm/min; ISO 527
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO Test
Charpy Impact Unnotched 6.00 J/cm²
28.6 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359
Melting Point 220 °C
428 °F
10 K/min
Electrical Properties Metric English Comments
Dielectric Constant 6.2

@Frequency 1.00e+6 Hz
6.2

@Frequency 1.00e+6 Hz
IEC 60250
Dissipation Factor 0.20

@Frequency 1.00e+6 Hz
0.20

@Frequency 1.00e+6 Hz
IEC 60250
Descriptive Properties Value Comments
Color BK30564
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding