| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Delrin® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Delrin® 100PE NC010 Acetal (POM)
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.19 g/cc | 0.0430 lb/in³ | |
| 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 | |
| Viscosity | 134900 cP @Shear Rate 5000 1/s, Temperature 230 °C |
134900 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
| 151800 cP @Shear Rate 5000 1/s, Temperature 215 °C |
151800 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 | |
| 167300 cP @Shear Rate 5000 1/s, Temperature 200 °C |
167300 cP @Shear Rate 5000 1/s, Temperature 392 °F |
ISO 11403-1 -2 | |
| 697800 cP @Shear Rate 500 1/s, Temperature 230 °C |
697800 cP @Shear Rate 500 1/s, Temperature 446 °F |
ISO 11403-1 -2 | |
| 779300 cP @Shear Rate 500 1/s, Temperature 215 °C |
779300 cP @Shear Rate 500 1/s, Temperature 419 °F |
ISO 11403-1 -2 | |
| 875100 cP @Shear Rate 500 1/s, Temperature 200 °C |
875100 cP @Shear Rate 500 1/s, Temperature 392 °F |
ISO 11403-1 -2 | |
| Linear Mold Shrinkage, Flow | 0.022 cm/cm | 0.022 in/in | ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
| Melt Flow | 2.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
| 2.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 91 | 91 | ISO 2039-2 |
| Hardness, Rockwell R | 121 | 121 | ISO 2039-2 |
| Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
| Elongation at Break | 45 % | 45 % | Nominal; ISO 527-1/-2 |
| Elongation at Yield | 26 % | 26 % | ISO 527-1/-2 |
| Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
| Flexural Strength | 79.0 MPa @Strain 3.50 % |
11500 psi @Strain 3.50 % |
ISO 178 |
| Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| 40.0 J/cm² @Temperature -30.0 °C |
190 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eA |
| 1.30 J/cm² @Temperature -30.0 °C |
6.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
| 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-1/-2 |
| 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 | |
| Melting Point | 178 °C | 352 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 157 °C | 315 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 99.0 °C | 210 °F | ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 3.00e+14 ohm | 3.00e+14 ohm | IEC 60093 |
| Dielectric Constant | 3.9 @Frequency 1.00e+6 Hz |
3.9 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 4.0 @Frequency 100 Hz |
4.0 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 44.0 kV/mm | 1120 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.00050 @Frequency 100 Hz |
0.00050 @Frequency 100 Hz |
IEC 60250 |
| 0.0050 @Frequency 1.00e+6 Hz |
0.0050 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additives | Release agent | |
| Delivery Form | Pellets | |
| Emissions | <2 mg/kg | VDA 275 |
| Part Marking Code | >POM< | ISO 11469 |
| Processing | Injection Moulding | |
| Other Extrusion | ||
| Profile Extrusion | ||
| Sheet Extrusion | ||
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | POM | ISO 1043 |