| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant |
| Manufacturer | E-Polymers Co. Ltd. |
| Trade Name | TEKASTER® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.67 g/cc | 0.0603 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 95 | 95 | ASTM D785 |
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 150 MPa | 21800 psi | ASTM D638 |
| Elongation at Break | 2.3 % | 2.3 % | ASTM D638 |
| Flexural Yield Strength | 230 MPa | 33400 psi | ASTM D790 |
| Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
| Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
| 0.800 J/cm @Temperature -40.0 °C |
1.50 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 254 °C | 489 °F | ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 225 °C | 437 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 33 % | 33 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 93 |
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 93 |
| Dielectric Constant | 3.8 @Frequency 1e+6 Hz |
3.8 @Frequency 1e+6 Hz |
IEC 250 |
| Dissipation Factor | 0.018 @Frequency 1e+6 Hz |
0.018 @Frequency 1e+6 Hz |
IEC 250 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
| Mold Temperature | 80.0 - 100 °C | 176 - 212 °F |