Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® XE 4181 nat PA1010.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grilamid XE 4181 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 natural is highly resistant to automotive fluids and chemicals in general. Unique features of Grilamid XE 4181 natural are: Polymer fully based on renewable raw materialsFlexibility, high elongationVery low water absorptionGood cold impact resistanceGood heat and UV resistanceExcellent chemical and zinc-chloride resistanceEasy processing Application examples: Grilamid XE 4181 natural has been designed for use in various types of demanding automotive and industrial tubings. It is technically a very close and bio based alternative to comparable PA12 based Grilamid products.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Water Absorption 1.3 %
1.3 %
ISO 62
Moisture Absorption 0.700 %
0.700 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
dry; ISO 527-1/-2
40.0 MPa
5800 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 30 %
30 %
conditioned; ISO 527-1/-2
30 %
30 %
dry; ISO 527-1/-2
Tensile Modulus 0.600 GPa
87.0 ksi
conditioned; ISO 527-1/-2
0.800 GPa
116 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
5.50 J/cm²

@Temperature 30.0 °C
26.2 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 170 µm/m-°C
94.4 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
Melting Point 197 °C
387 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
conditioned; IEC 60093
1.00e+11 ohm-cm
1.00e+11 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 37.0 kV/mm
940 kV/in
conditioned; IEC 60243-1
39.0 kV/mm
991 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Air intake sytems
Compressed air systems
Fuel systems
Hydraulic systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Product Attributes Bio based Polyamide
Flexible
High viscosity
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)
Users viewing this material also viewed the following: