| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Optical Grade |
| Manufacturer | Entec Engineered Resins |
| Trade Name | Hylex® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Entec Hylex® P1310L1 HB Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ASTM D792 |
| Water Absorption at Saturation | 0.15 % | 0.15 % | Immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.005 - 0.007 cm/cm | 0.005 - 0.007 in/in | ASTM D955 |
| Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 72 | 72 | ASTM D785 |
| Tensile Strength at Break | 68.9 MPa | 10000 psi | ASTM D638 |
| Elongation at Break | 130 % | 130 % | ASTM D638 |
| Flexural Strength | 96.5 MPa | 14000 psi | ASTM D790 |
| Flexural Modulus | 2.34 GPa | 340 ksi | ASTM D790 |
| Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 139 °C | 282 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 132 °C | 270 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
|
| HB @Thickness 3.00 mm |
HB @Thickness 0.118 in |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.586 | 1.586 | ASTM D542 |
| Haze | 1.0 % | 1.0 % | ASTM D1003 |
| Transmission, Visible | 88 % | 88 % | ASTM D1003 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.0e+17 ohm-cm | 1.0e+17 ohm-cm | ASTM D257 |
| Dielectric Strength | 15.0 kV/mm | 380 kV/in | ASTM D149 |