| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
| Manufacturer | LG Chemical |
| Trade Name | Lupox® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical Lupox® GP2306FG PBT+GF30%.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.62 g/cc | 1.62 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.020 | 0.020 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.010 cm/cm @Thickness 3.20 mm |
0.0030 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 125 MPa @Thickness 3.20 mm |
18100 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 3.0 % @Thickness 3.20 mm |
3.0 % @Thickness 0.126 in |
5mm/min; ASTM D638 |
| Flexural Yield Strength | 188 MPa @Thickness 3.20 mm |
27300 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Flexural Modulus | 8.34 GPa @Thickness 3.20 mm |
1210 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Izod Impact, Notched | 0.637 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 225 °C | 437 °F | @ Break; ASTM D3418 |
| Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 6.40 mm |
419 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C @Thickness 6.40 mm |
392 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
| 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
||
| 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
| 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
||
| 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 140 °C @Thickness >=0.710 mm |
284 °F @Thickness >=0.0280 in |
|
| 140 °C @Thickness >=1.50 mm |
284 °F @Thickness >=0.0591 in |
||
| 140 °C @Thickness >=3.00 mm |
284 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | V-0 @Thickness >=0.710 mm |
V-0 @Thickness >=0.0280 in |
|
| V-0 @Thickness >=1.50 mm |
V-0 @Thickness >=0.0591 in |
||
| V-0 @Thickness >=3.00 mm |
V-0 @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | ASTM D257 |
| Dielectric Strength | 28.0 kV/mm @Thickness 1.00 mm |
711 kV/in @Thickness 0.0394 in |
ASTM D149 |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | |
| Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.710 mm |
7.0 - 15 sec @Thickness >=0.0280 in |
|
| 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
||
| High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 0.710 mm |
60 - 120 arcs @Thickness 0.0280 in |
|
| 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 235 - 250 °C | 455 - 482 °F | Injection Molding |
| Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
| Front Barrel Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
| Nozzle Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
| Melt Temperature | 245 - 255 °C | 473 - 491 °F | Injection Molding |
| Mold Temperature | 60.0 - 100 °C | 140 - 212 °F | Injection Molding |
| Drying Temperature | 120 °C | 248 °F | Injection Molding |
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |