| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | LTL Color Compounds |
| Trade Name | ColorFast® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.37 g/cc | 1.37 g/cc | ASTM D792 |
| Water Absorption | 1.5 % | 1.5 % | @ 24 Hours; ASTM D570 |
| Linear Mold Shrinkage | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | 0.125; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 172 MPa | 25000 psi | 2.0 in/min; ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | 2.0 in/min; ASTM D638 |
| Elongation at Yield | 2.0 % | 2.0 % | 2.0 in/min; ASTM D638 |
| Flexural Strength | 248 MPa | 36000 psi | 2.0 in/min; ASTM D790 |
| Flexural Modulus | 8.27 GPa | 1200 ksi | 2.0 in/min; ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 249 °C | 480 °F | Unannealed (0.250"); ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
| Middle Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
| Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
| Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
| Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
| Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
| Drying Temperature | 82.2 °C | 180 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | nominal; maximum drying time of 8 hours |
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
| Shot Size | 30 - 60 % | 30 - 60 % | |
| Vent Depth | 0.00381 - 0.00762 cm | 0.00150 - 0.00300 in | |
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm |