| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Gravi-Tech™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.69 g/cc | 2.69 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.011 cm/cm | 0.0080 - 0.011 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 113 @Temperature 23.0 °C |
113 @Temperature 73.4 °F |
ASTM D785 |
| Tensile Strength, Yield | 62.1 MPa | 9010 psi | Type I, 5.1 mm/min; ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | Type I, 5.1 mm/min; ASTM D638 |
| Tensile Modulus | 5.52 GPa | 801 ksi | Type I, 5.1 mm/min; ASTM D638 |
| Flexural Strength | 103 MPa | 14900 psi | 1.3 mm/min; ASTM D790 |
| Flexural Modulus | 4.48 GPa | 650 ksi | 1.3 mm/min; ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Izod Impact, Unnotched | 4.30 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 188 °C | 370 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | Unannealed; ASTM D648 |
| Vicat Softening Point | 212 °C | 414 °F | ASTM D1525 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
| Mold Temperature | 82.2 - 135 °C | 180 - 275 °F | |
| Drying Temperature | 79.4 °C | 175 °F | |
| Dry Time | 4.00 hour | 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black | |
| Features | High Specific Gravity | |
| Non-Toxic | ||
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Appliance Components | |
| Automotive Applications | ||
| Consumer Applications | ||
| Handles | ||
| Industrial Applications | ||
| Knobs | ||
| Medical/Healthcare Applications | ||
| Metal Replacement | ||
| Sporting Goods | ||
| Weighting & Balancing |