Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S RV500 (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S RV500 (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
(Dry)
Water Absorption 4.8 %
4.8 %
initially dry
Moisture Absorption at Equilibrium 1.4 %
1.4 %
initially dry
Viscosity Measurement 140
140
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
Elongation at Break 3.1 %
3.1 %
Tensile Modulus 11.5 GPa
1670 ksi
Charpy Impact Unnotched 11.0 J/cm²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V